5.0 g / 10 min (Test Method: ASTM D1238 190C @ 2.16kg)
0.934 g / cm3 (Test Method: ASTM D1505)
UL00514 isa copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 250°C(482°F) may cause resin degradation.